Mechanical Properties Metric English Comments
Izod Impact, Notched 0.128 J/cm
0.240 ft-lb/in
Tra-Con Tra-Bond 2113 Clear Low Viscosity Epoxy Adhesive
TRA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to gla..
Izod Impact, Notched 0.128 J/cm
0.240 ft-lb/in
Tra-Con Tra-Bond 216L01 Clear Low Viscosity Epoxy Adhesive
TRA-BOND 216L01 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to g..
Izod Impact, Notched 0.128 J/cm
0.240 ft-lb/in
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms..
Izod Impact, Notched 0.128 J/cm
0.240 ft-lb/in
Atom Adhesives AA-BOND 2113 Epoxy Adhesive
AA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flow ability and wetting characteristics, and adheres strongly to gla..