Polymer Property : Izod Impact, Notched = 0.184 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.184 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.345 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Therma-Tech™ NJC-7500 Nylon 12  (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.184 J/cm
0.345 ft-lb/in
ASTM D256
Plenco 2308 Phenolic, Granular, Transfer Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Izod Impact, Notched 0.184 J/cm
0.345 ft-lb/in
ASTM D256
Plenco 2482 Phenolic, Granular, Transfer Molded
PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized ..
Izod Impact, Notched 0.184 J/cm
0.345 ft-lb/in
ASTM D256
Plenco 3356 Phenolic, Granular, Compression Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..