POLYMER SEARCH
Polymer Property : Charpy Impact, Notched = 9.76 ft-lb/in²
Polymer Property :
Charpy Impact, Notched =
9.76 ft-lb/in²
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Charpy Impact, Notched
2.05
J/cm²
9.76
ft-lb/in²
ISO 179
Chi Mei Kibilac® PW-997S ASA Polymer