Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 8.90 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 8.90 J/cm²
42.4 ft-lb/in²
ISO 179
Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin
Extrusion molding, blow molding and thick-wall injection molding grade. It has a improved mold release property and is bluish-tinted to exhibit clear color.Applications:Extruded products such as she..
Copyright © lookpolymers.com All Rights Reserved