Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.82 J/cm² | 8.66 ft-lb/in² | |
Eastman Tenite 358-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 1.82 J/cm² @Temperature 23.0 °C |
8.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.82 J/cm² @Temperature -30.0 °C |
8.66 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema. |