Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | Partial Break; ISO 179/1eA |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179 |
Styrolution Styrolux BX6400 SBC Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179/2fn |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179/2fn |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179/2fn |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | |
BASF Novolen® 2900 NC Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |