Polymer Property : Charpy Impact, Notched = 7.76 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.63 J/cm²
7.76 ft-lb/in²
Eastman Tenite 130-33 Cellulose Acetate  (discontinued **)
33% Plasticized, contains 100% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.63 J/cm²
7.76 ft-lb/in²
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..