Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179 |
Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin Standard injection molding grade that has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, electric, electronic, medical, safety a.. |
|||
Charpy Impact, Notched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179 |
Teijin Panlite® L-1250Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has normal fluidity and weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, elect.. |
|||
Charpy Impact, Notched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179 |
Teijin Panlite® L-1250ZW Extrusion Grade Polycarbonate Resin Information provided by Teijin Chemicals Ltd. |
|||
Charpy Impact, Notched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179 |
Teijin Panlite® LV-2250Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required for normal fluidity.Applications:.. |
|||
Charpy Impact, Notched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179 |
Teijin Panlite® LV-2250Z Transparent and Weather Resistant grade Polycarbonate Resin Typical injection molding grade that has weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of electric, electronic, business machine and industrial equipment com.. |