Polymer Property : Charpy Impact, Notched = 5.85 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.23 J/cm²
5.85 ft-lb/in²
ISO 179
Chi Mei Kibilac® PW-957 ASA Polymer
Injection
Charpy Impact, Notched 1.23 J/cm²
5.85 ft-lb/in²
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Charpy Impact, Notched 1.23 J/cm²

@Temperature -40.0 °C
5.85 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuP..
Copyright © lookpolymers.com All Rights Reserved