Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.77 J/cm² | 27.5 ft-lb/in² | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |