Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.350 - 1.10 J/cm² | 1.67 - 5.24 ft-lb/in² | Average value: 0.636 J/cm² Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Charpy Impact, Notched | 0.700 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.909 J/cm² Grade Count:11 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.250 - 1.10 J/cm² | 1.19 - 5.24 ft-lb/in² | Average value: 0.582 J/cm² Grade Count:4 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Charpy Impact, Notched | 0.500 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.700 J/cm² Grade Count:6 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.700 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.960 J/cm² Grade Count:5 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact, Notched | 0.600 - 1.10 J/cm² @Temperature -30.0 - 0.000 °C |
2.86 - 5.24 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 0.902 J/cm² Grade Count:14 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 1.00 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.03 J/cm² Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.250 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
1.19 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.629 J/cm² Grade Count:7 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.470 - 1.10 J/cm² | 2.24 - 5.24 ft-lb/in² | Average value: 0.769 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Charpy Impact, Notched | 0.600 - 1.10 J/cm² @Temperature -40.0 - -30.0 °C |
2.86 - 5.24 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.921 J/cm² Grade Count:11 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |