Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.04 J/cm²
4.95 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66
Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 1.04 J/cm²

@Temperature -30.0 °C
4.95 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.