Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.02 J/cm² | 4.85 ft-lb/in² | |
Eastman Tenite 132E-28 Cellulose Acetate
(discontinued **) 28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 1.02 J/cm² @Temperature 23.0 °C |
4.85 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.02 J/cm² | 4.85 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 7400F Polybutylene Terephthalate (PBT), Low friction, Low wear, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 1.02 J/cm² @Temperature -30.0 °C |
4.85 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Charpy Impact, Notched | 1.02 J/cm² @Temperature -30.0 °C |
4.85 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Charpy Impact, Notched | 1.02 - 1.83 J/cm² | 4.85 - 8.71 ft-lb/in² | Average value: 1.54 J/cm² Grade Count:7 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |