Polymer Property : Charpy Impact, Notched = 4.43 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.930 J/cm²
4.43 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Charpy Impact, Notched 0.930 J/cm²
4.43 ft-lb/in²
ISO 179/1eA
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Charpy Impact, Notched 0.930 J/cm²
4.43 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Charpy Impact, Notched 0.930 J/cm²
4.43 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro..
Charpy Impact, Notched 0.930 J/cm²
4.43 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Charpy Impact, Notched 0.930 J/cm²

@Temperature 23.0 °C
4.43 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT™ 2011 Polyimide (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...