Polymer Property : Charpy Impact, Notched = 2.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.60 - 2.60 J/cm²
7.61 - 12.4 ft-lb/in²
Average value: 2.00 J/cm² Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Charpy Impact, Notched 0.200 - 2.60 J/cm²

@Temperature -20.0 - -20.0 °C
0.952 - 12.4 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 1.39 J/cm² Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.200 - 2.60 J/cm²

@Thickness 102 - 102 mm
0.952 - 12.4 ft-lb/in²

@Thickness 4.00 - 4.00 in
Average value: 1.39 J/cm² Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..