Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.90 J/cm² @Temperature -30.0 °C |
18.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Charpy Impact, Notched | 3.90 J/cm² | 18.6 ft-lb/in² | |
Ineos ABS Lustran® 648 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 3.90 J/cm² @Temperature -30.0 °C |
18.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |