Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 - 2.50 J/cm² | 1.90 - 11.9 ft-lb/in² | ISO.179 DN.53453 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Charpy Impact, Notched | 0.250 - 2.50 J/cm² @Temperature -30.0 - -20.0 °C |
1.19 - 11.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.841 J/cm² Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Charpy Impact, Notched | 0.500 - 2.50 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 11.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.08 J/cm² Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.900 - 2.50 J/cm² @Temperature -40.0 - -20.0 °C |
4.28 - 11.9 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.52 J/cm² Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.400 - 2.50 J/cm² | 1.90 - 11.9 ft-lb/in² | ISO.179 DN.53453 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Charpy Impact, Notched | 0.100 - 2.50 J/cm² | 0.476 - 11.9 ft-lb/in² | Average value: 0.992 J/cm² Grade Count:68 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.500 - 2.50 J/cm² @Temperature -30.0 - -20.0 °C |
2.38 - 11.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.49 J/cm² Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.200 - 2.50 J/cm² @Temperature -30.0 - 30.0 °C |
0.952 - 11.9 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.832 J/cm² Grade Count:29 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Charpy Impact, Notched | 0.650 - 2.50 J/cm² | 3.09 - 11.9 ft-lb/in² | Average value: 1.62 J/cm² Grade Count:20 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact, Notched | 1.20 - 2.50 J/cm² | 5.71 - 11.9 ft-lb/in² | Average value: 1.84 J/cm² Grade Count:21 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact, Notched | 0.800 - 2.50 J/cm² | 3.81 - 11.9 ft-lb/in² | Average value: 1.40 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Charpy Impact, Notched | 0.700 - 2.50 J/cm² | 3.33 - 11.9 ft-lb/in² | Average value: 1.62 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.800 - 2.50 J/cm² | 3.81 - 11.9 ft-lb/in² | Average value: 1.72 J/cm² Grade Count:6 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |