Polymer Property : Charpy Impact, Notched = 1.82 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.82 J/cm²
8.66 ft-lb/in²
Eastman Tenite 358-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.82 J/cm²

@Temperature 23.0 °C
8.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.82 J/cm²

@Temperature -30.0 °C
8.66 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema.