Polymer Property : Charpy Impact, Notched = 1.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.300 - 1.50 J/cm²
1.43 - 7.14 ft-lb/in²
Average value: 0.892 J/cm² Grade Count:90
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 1.00 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
4.76 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.33 J/cm² Grade Count:2
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Charpy Impact, Notched 0.350 - 1.50 J/cm²
1.67 - 7.14 ft-lb/in²
Average value: 0.700 J/cm² Grade Count:16
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact, Notched 0.600 - 1.50 J/cm²

@Temperature -30.0 - 30.0 °C
2.86 - 7.14 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.27 J/cm² Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Charpy Impact, Notched 0.400 - 1.50 J/cm²

@Temperature -30.0 - -20.0 °C
1.90 - 7.14 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.800 J/cm² Grade Count:3
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.300 - 1.50 J/cm²

@Temperature -40.0 - -20.0 °C
1.43 - 7.14 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.01 J/cm² Grade Count:8
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Charpy Impact, Notched 0.350 - 1.50 J/cm²
1.67 - 7.14 ft-lb/in²
Average value: 1.08 J/cm² Grade Count:19
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.400 - 1.50 J/cm²
1.90 - 7.14 ft-lb/in²
Average value: 0.981 J/cm² Grade Count:24
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Charpy Impact, Notched 0.200 - 1.50 J/cm²
0.952 - 7.14 ft-lb/in²
Average value: 0.533 J/cm² Grade Count:11
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 1.20 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.38 J/cm² Grade Count:2
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.400 - 1.50 J/cm²
1.90 - 7.14 ft-lb/in²
Average value: 1.07 J/cm² Grade Count:11
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.700 - 1.50 J/cm²
3.33 - 7.14 ft-lb/in²
Average value: 1.15 J/cm² Grade Count:4
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Charpy Impact, Notched 0.500 - 1.50 J/cm²
2.38 - 7.14 ft-lb/in²
Average value: 0.867 J/cm² Grade Count:6
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
Charpy Impact, Notched 0.300 - 1.50 J/cm²
1.43 - 7.14 ft-lb/in²
Average value: 0.923 J/cm² Grade Count:7
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Charpy Impact, Notched 0.300 - 1.50 J/cm²
1.43 - 7.14 ft-lb/in²
Average value: 0.879 J/cm² Grade Count:37
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Charpy Impact, Notched 0.500 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J/cm² Grade Count:2
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.700 - 1.50 J/cm²
3.33 - 7.14 ft-lb/in²
Average value: 1.20 J/cm² Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Charpy Impact, Notched 1.50 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
7.14 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.50 J/cm² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Charpy Impact, Notched 0.300 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.614 J/cm² Grade Count:84
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Charpy Impact, Notched 0.250 - 1.50 J/cm²
1.19 - 7.14 ft-lb/in²
Average value: 0.882 J/cm² Grade Count:11
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..