Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.280 - 1.00 J/cm²

@Temperature -40.0 - 30.0 °C
1.33 - 4.76 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 0.693 J/cm² Grade Count:68
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for ..
Charpy Impact, Notched 0.280 - 0.600 J/cm²
1.33 - 2.86 ft-lb/in²
Average value: 0.398 J/cm² Grade Count:6
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact, Notched 0.280 J/cm²

@Temperature -23.0 °C
1.33 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Global PP-1126-NK Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation.
Charpy Impact, Notched 0.280 J/cm²

@Temperature 23.0 °C
1.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
LATI Latilub 66-20T PA66, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179-1
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179-1
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic
Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179
Polyram RamOfin PPH343T4BK10 Polypropylene, 20% Mineral Filled
20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram.
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA)
High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179
Chi Mei Kibiton® PB-5903 SBC
High transparency, high toughness, PS Impact modifier
Charpy Impact, Notched 0.280 J/cm²

@Temperature 23.0 °C
1.33 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT™ 2062 Polyimide, Anthrazit Gleamy, 15% Graphite, 10% PTFE (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Charpy Impact, Notched 0.280 J/cm²

@Temperature -40.0 °C
1.33 ft-lb/in²

@Temperature -40.0 °F
ISO R179
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Charpy Impact, Notched >= 0.280 J/cm²

@Temperature 23.0 °C
>= 1.33 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched >= 0.280 J/cm²

@Temperature 23.0 °C
>= 1.33 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPH BL5003 Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact, Notched 0.280 - 1.40 J/cm²
1.33 - 6.66 ft-lb/in²
Average value: 0.715 J/cm² Grade Count:11
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179
Polyram RamOfin PPH343T4BK11 Polypropylene, 20% Mineral Filled
20% Mineral filled, UV stabilized, heat resistant polypropylene for injection molding applications.Information provided by Polyram.
Charpy Impact, Notched 0.280 - 3.90 J/cm²
1.33 - 18.6 ft-lb/in²
Average value: 1.57 J/cm² Grade Count:99
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Copyright © lookpolymers.com All Rights Reserved