Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.252 J/cm²

@Temperature 22.8 °C
1.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ LNU 012 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with good heat resistance and good surface finish designed for fast injection molding of large electrical appliance parts.Availability..