Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.350 - 1.10 J/cm²
1.67 - 5.24 ft-lb/in²
Average value: 0.636 J/cm² Grade Count:12
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Charpy Impact, Notched 0.700 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.909 J/cm² Grade Count:11
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.250 - 1.10 J/cm²
1.19 - 5.24 ft-lb/in²
Average value: 0.582 J/cm² Grade Count:4
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Charpy Impact, Notched 0.500 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:6
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.700 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.960 J/cm² Grade Count:5
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Charpy Impact, Notched 0.600 - 1.10 J/cm²

@Temperature -30.0 - 0.000 °C
2.86 - 5.24 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 0.902 J/cm² Grade Count:14
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact, Notched 1.00 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
4.76 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.03 J/cm² Grade Count:6
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.250 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
1.19 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.629 J/cm² Grade Count:7
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.470 - 1.10 J/cm²
2.24 - 5.24 ft-lb/in²
Average value: 0.769 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Charpy Impact, Notched 0.600 - 1.10 J/cm²

@Temperature -40.0 - -30.0 °C
2.86 - 5.24 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.921 J/cm² Grade Count:11
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..