Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.07 J/cm² | 5.09 ft-lb/in² | |
Ineos ABS Centrex® 485 ASA+AES Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformingInformation provided by Bayer Pol.. |
|||
Charpy Impact, Notched | 1.07 J/cm² | 5.09 ft-lb/in² | |
Arkema Group Lucalor® PEY 436 CPVC, Pipe Grade LUCALOR PEY 436 is a chlorinated polyvinyl chloride compound (CPVC) developed for the extrusion of pipes for hot water supply and distribution systems.ISO data provided by the manufacturer, Arkema. |