Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.04 J/cm² | 4.95 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 1.04 J/cm² @Temperature -30.0 °C |
4.95 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |