Polymer Property : Charpy Impact, Notched = 0.910 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.910 J/cm²
4.33 ft-lb/in²
Conditioned; ISO 179/1eA
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p..
Charpy Impact, Notched 0.910 J/cm²
4.33 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66
Applications: Framework of CoilsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 0.910 J/cm²

@Temperature -30.0 °C
4.33 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..
Charpy Impact, Notched 0.910 J/cm²

@Temperature -30.0 °C
4.33 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Charpy Impact, Notched 0.910 J/cm²

@Temperature -30.0 °C
4.33 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Conditioned)
Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:..