Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.190 - 0.390 J/cm²
0.904 - 1.86 ft-lb/in²
Average value: 0.305 J/cm² Grade Count:13
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ASTM D256
Plenco 2424 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical ..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a ..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ASTM D256
Plenco 2300 Phenolic, Granular, Compression Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ASTM D256
Plenco 2571 Phenolic, Granular, Injection Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ISO 179
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA)
Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Charpy Impact, Notched 0.190 J/cm²

@Temperature -30.0 °C
0.904 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 H Polypropylene
Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF.