Polymer Property : Charpy Impact, Notched = 0.820 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179
GEHR Plastics PEEK Polyetheretherketone
Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment...
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66
Applications: Connector AS PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 0.820 J/cm²

@Temperature -30.0 °C
3.90 ft-lb/in²

@Temperature -22.0 °F
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V..
Charpy Impact, Notched 0.820 J/cm²

@Temperature -30.0 °C
3.90 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned)
Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi..
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad..