Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.680 J/cm² | 3.24 ft-lb/in² | ISO 179/1eA |
Radici Radilon® S35HR (dry) Nylon 6 Medium high viscosityInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.680 J/cm² | 3.24 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact, Notched | 0.680 J/cm² | 3.24 ft-lb/in² | Complete Break; ISO 179 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Charpy Impact, Notched | 0.680 J/cm² | 3.24 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Charpy Impact, Notched | 0.680 J/cm² | 3.24 ft-lb/in² | |
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Charpy Impact, Notched | 0.680 J/cm² @Temperature -30.0 °C |
3.24 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |