Polymer Property : Charpy Impact, Notched = 0.198 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.198 J/cm²
0.942 ft-lb/in²
ASTM D256
Plenco 2482 Phenolic, Granular, Transfer Molded
PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized ..