Polymer Property : Charpy Impact, Notched = 0.100 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..