Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.345 MPa @Strain 8.00 % |
50.0 psi @Strain 8.00 % |
Load applied parallel to fiber plane |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.345 MPa @Strain 8.00 % |
50.0 psi @Strain 8.00 % |
Load applied parallel to fiber plane |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.345 MPa @Strain 40.0 % |
50.0 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® HD60 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.345 MPa @Strain 2.00 % |
50.0 psi @Strain 2.00 % |
Load applied normal to fiber plane |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Compressive Yield Strength | 0.345 MPa @Strain 2.00 % |
50.0 psi @Strain 2.00 % |
Load applied parallel to fiber plane |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |