Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 84.0 - 250 MPa | 12200 - 36300 psi | Average value: 180 MPa Grade Count:22 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Ball Indentation Hardness | 84.0 MPa | 12200 psi | H358/30; ISO 2039-1 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Ball Indentation Hardness | 84.0 MPa @Load 36.5 kg, Time 30.0 sec |
12200 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Ball Indentation Hardness | 84.0 MPa @Load 36.5 kg, Time 30.0 sec |
12200 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |