Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 65.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 65.0 MPa
9430 psi
ISO 2039-1
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)
Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan..
Ball Indentation Hardness 65.0 - 105 MPa
9430 - 15200 psi
Average value: 90.0 MPa Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Ball Indentation Hardness 65.0 MPa
9430 psi
ISO 2039-1
Ineos ABS Lustran® ABS E112LG Pellets
Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles.
Ball Indentation Hardness 65.0 MPa

@Load 36.5 kg,
Time 30.0 sec
9430 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 796 M Colored ASA
Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Ball Indentation Hardness 65.0 MPa

@Load 36.5 kg,
Time 30.0 sec
9430 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 797 S UV White 33999 Q455 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Ball Indentation Hardness 65.0 MPa

@Load 36.5 kg,
Time 30.0 sec
9430 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Ball Indentation Hardness 65.0 MPa
9430 psi
ISO 2039-1
Styrolution PS 2710 HIPS
Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr..
Ball Indentation Hardness 65.0 MPa
9430 psi
358 N/30s; ISO 2039
Borealis HB601WG Polypropylene Homopolymer
HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent ..
Ball Indentation Hardness 65.0 MPa
9430 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSS/4 LF 1 PA666
Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import..
Ball Indentation Hardness 65.0 MPa
9430 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSS/4 LF 2 PA666
Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import..
Ball Indentation Hardness 65.0 MPa
9430 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSS/4 PA666
Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas..
Ball Indentation Hardness 65.0 MPa

@Load 36.5 kg,
Time 30.0 sec
9430 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2650 Z6 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF
Ball Indentation Hardness 65.0 - 70.0 MPa
9430 - 10200 psi
DIN 53 456
Isoflon PCTFE Polychlorotrifluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Ball Indentation Hardness 65.0 MPa
9430 psi
Fm=358N; Ø 50x4mm; ISO 2039-1
SYNTHOS Krasten® 562E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo..
Copyright © lookpolymers.com All Rights Reserved