Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 34800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 240 MPa

@Load 36.5 kg,
Time 30.0 sec
34800 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® 378 P G7 35% Glass Filled SAN
Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Ball Indentation Hardness 240 MPa
34800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-35 PA6-GF35
Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy..
Ball Indentation Hardness 240 MPa
34800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
Ball Indentation Hardness 240 MPa
34800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
Ball Indentation Hardness 240 MPa
34800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
Ball Indentation Hardness 240 MPa
34800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60
Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p..
Ball Indentation Hardness 240 MPa
34800 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30
Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X..
Ball Indentation Hardness 240 MPa
34800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30
Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X..
Ball Indentation Hardness 240 MPa
34800 psi
(H 961/30); ISO 2039-1
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Ball Indentation Hardness 240 MPa
34800 psi
H 961/30; ISO 32039-1
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Ball Indentation Hardness 240 MPa
34800 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber
This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB..
Ball Indentation Hardness 240 MPa
34800 psi
H 961/30; ISO 2039-1
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..