Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 29700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 205 MPa
29700 psi
ISO 2039-1
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 205 MPa
29700 psi
ISO 2039-1
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data)
This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi..
Ball Indentation Hardness 205 MPa
29700 psi
ISO 2039-1
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Ball Indentation Hardness 205 MPa
29700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30
Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr..
Ball Indentation Hardness 205 MPa
29700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30
Information provided by EMS Grivory
Ball Indentation Hardness 205 MPa
29700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30
Information provided by EMS Grivory
Ball Indentation Hardness 205 MPa
29700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50
Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p..
Ball Indentation Hardness 205 MPa

@Load 98.0 kg,
Time 30.0 sec
29700 psi

@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Ball Indentation Hardness 205 MPa

@Load 36.5 kg
29700 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Ball Indentation Hardness 205 MPa

@Load 36.5 kg
29700 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
Ball Indentation Hardness 205 MPa
29700 psi
ISO 2039-1
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.