Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 290 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 140 - 290 MPa
20300 - 42100 psi
Average value: 237 MPa Grade Count:20
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Ball Indentation Hardness 75.0 - 290 MPa
10900 - 42100 psi
Average value: 160 MPa Grade Count:19
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Ball Indentation Hardness 270 - 290 MPa
39200 - 42100 psi
Average value: 283 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..