Polymer Property : Ball Indentation Hardness = 235 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 235 MPa
34100 psi
ISO 2039-1
Polycasa XT PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Ball Indentation Hardness 235 MPa
34100 psi
ISO 2039-1
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data)
Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good ..
Ball Indentation Hardness 235 MPa
34100 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50
Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c..
Ball Indentation Hardness 235 MPa
34100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam..
Ball Indentation Hardness 235 MPa
34100 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam..
Ball Indentation Hardness 235 MPa
34100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30
Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid..
Ball Indentation Hardness 235 MPa
34100 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30
Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid..