Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 154 MPa @Load 36.5 kg, Time 30.0 sec |
22300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Ball Indentation Hardness | 154 MPa @Load 36.5 kg, Time 30.0 sec |
22300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Ball Indentation Hardness | 154 MPa | 22300 psi | ISO 2039-1 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Ball Indentation Hardness | 154 MPa | 22300 psi | ISO 2039-1 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Ball Indentation Hardness | 154 MPa | 22300 psi | ISO 2039-1 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Ball Indentation Hardness | 154 MPa @Load 36.5 kg, Time 30.0 sec |
22300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Ball Indentation Hardness | 154 MPa @Load 36.5 kg, Time 30.0 sec |
22300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Ball Indentation Hardness | 154 - 224 MPa | 22300 - 32500 psi | Average value: 174 MPa Grade Count:12 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |