Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 148 MPa | 21500 psi | ISO 2039-1 |
Nilit FRIANYL B63 MG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 148 MPa | 21500 psi | ISO 2039-1 |
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit.. |