Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO2039.1 DIN.53456 |
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptan.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PSU Polysulphone It is a non-reinforced amorphous polymer whose main features are its high thermal, electrical and mechanical properties which are typical of a crystalline polymer. Compared to its "brother" PES it h.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL B63 KG20 Nylon 6 for injection molding, 20% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Ball Indentation Hardness | 140 - 155 MPa | 20300 - 22500 psi | ISO.2039-2 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL B63 TF-GV 1520 Nylon 6 for injection molding, 15% PTFE lubricated, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS/2 FA PA666 Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow .. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 LF 2 PA666 Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BR 40 PA6 Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie.. |
|||
Ball Indentation Hardness | 140 MPa @Load 36.5 kg |
20300 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 TF10 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 POM Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 400 LS POM Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Ball Indentation Hardness | 140 MPa @Load 36.5 kg |
20300 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
CENTROPLAST CENTRODAL W Polyoxymethylene POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe.. |