Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 140 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Ball Indentation Hardness 140 MPa
20300 psi
ISO2039.1 DIN.53456
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer
Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptan..
Ball Indentation Hardness 140 - 155 MPa
20300 - 22500 psi
ISO.2039-2
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL A63 W Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL B63 KG20 Nylon 6 for injection molding, 20% chalk filled
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data)
Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos..
Ball Indentation Hardness 140 - 155 MPa
20300 - 22500 psi
ISO.2039-2
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL A63 GV 5 Nylon 6.6 for injection molding, 5% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Nilit FRIANYL B63 TF-GV 1520 Nylon 6 for injection molding, 15% PTFE lubricated, 20% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 140 - 290 MPa
20300 - 42100 psi
Average value: 237 MPa Grade Count:20
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade
PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS.
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® AS LF 20 PA66-Z20
Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert..
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BS/2 PA6
Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior..
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc..
Ball Indentation Hardness 140 MPa
20300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc..
Ball Indentation Hardness 140 MPa
20300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGZ-50 PA666-GF50
Information provided by EMS Grivory
Ball Indentation Hardness 140 MPa
20300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BG-50 HM PA6-GF50
Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop..
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BR 40 PA6
Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie..
Ball Indentation Hardness 140 MPa

@Load 36.5 kg
20300 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 TF10 Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Ball Indentation Hardness 140 MPa
20300 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 POM
Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 140 MPa
20300 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 400 LS POM
Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 140 MPa
20300 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 400 POM
Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
Ball Indentation Hardness 140 MPa

@Load 36.5 kg,
Time 30.0 sec
20300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Ball Indentation Hardness 140 MPa

@Load 36.5 kg
20300 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Ball Indentation Hardness 140 MPa
20300 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an..
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
CENTROPLAST CENTRODAL W Polyoxymethylene
POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe..
Copyright © lookpolymers.com All Rights Reserved