Polymer Property : Ball Indentation Hardness = 13200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 91.0 MPa
13200 psi
ISO 2039-1
Nilit RECONYL B S20 Recycled nylon 6 for injection molding
Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 91.0 MPa
13200 psi
358 N/30s; ISO 2039
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Ball Indentation Hardness 91.0 MPa
13200 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact