Polymer Property : Ball Indentation Hardness = 118 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 118 MPa
17100 psi
ISO 2039-1
Nilit RECONYL B S Recycled nylon 6 for injection molding
Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 118 MPa
17100 psi
ISO 2039-1
Nilit FRIANYL A63 HS-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 118 MPa
17100 psi
ISO 2039-1
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..