Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PC Polycarbonate This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does ma.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Nilit FRIANYL A63 S15 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Nilit FRIANYL C73 HS-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 110 - 211 MPa | 16000 - 30600 psi | Average value: 174 MPa Grade Count:3 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Ball Indentation Hardness | 110 - 120 MPa | 16000 - 17400 psi | Average value: 115 MPa Grade Count:7 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039 |
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 110 MPa @Load 36.5 kg, Time 30.0 sec |
16000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S KR 2863 C Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Ball Indentation Hardness | 110 MPa @Load 36.5 kg, Time 30.0 sec |
16000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Ball Indentation Hardness | 110 MPa @Load 36.5 kg, Time 30.0 sec |
16000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S KR 2864 C UV Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | ISO 2039-1 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-23H PA12-GF23 Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Ball Indentation Hardness | 110 - 150 MPa | 16000 - 21800 psi | ISO 2032 |
Adamas Adalon® 466 PTFE, Mineral/Organic Filler Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |
|||
Ball Indentation Hardness | 110 - 115 MPa | 16000 - 16700 psi | Average value: 113 MPa Grade Count:3 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Ball Indentation Hardness | 110 MPa @Load 36.5 kg, Time 30.0 sec |
16000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S KR 2863 C UV Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Ball Indentation Hardness | 110 MPa | 16000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |
|||
Ball Indentation Hardness | 110 - 132 MPa | 16000 - 19100 psi | Average value: 117 MPa Grade Count:7 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |