Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 12.99 J | 9.583 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |