Polymer Property : Gardner Impact = 9.04 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 9.04 J

@Thickness 3.17 mm
6.67 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Gardner Impact 9.04 J

@Thickness 3.17 mm
6.67 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Gardner Impact 9.04 J

@Thickness 3.17 mm
6.67 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Gardner Impact 9.04 J

@Thickness 3.17 mm
6.67 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Gardner Impact 9.04 J
6.67 ft-lb
ASTM D5420
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..