Mechanical Properties Metric English Comments
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 3216 CUW BLK Polypropylene
Multi-Pro 3216 CUW BLK is well suited for resin furniture requiring high impact strength and stiffness at moderate cost.Data provided by Multibase.
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 4013 CU Yellow 40% Filler Content Polypropylene
Data provided by Multibase.
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D5420
PolyOne OnForce™ LFT AM-40LGF/001 Natural Polyphthalamide (PPA)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D3029
Polymer Resources PC-HH Polycarbonate, High Heat
Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource..
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D3029
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized
Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Gardner Impact >= 11.3 J
>= 8.33 ft-lb
Buckeye Polymers BP PPC 0212 R Reprocessed Polypropylene, Unfilled
Blk/WhiteThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds ar..
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D3029
Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 4012 C Polypropylene, 40% Mineral Filled
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag..