Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 9.04 J @Thickness 3.17 mm |
6.67 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Gardner Impact | 9.04 J @Thickness 3.17 mm |
6.67 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 9.04 J @Thickness 3.17 mm |
6.67 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Gardner Impact | 9.04 J @Thickness 3.17 mm |
6.67 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Gardner Impact | 9.04 J | 6.67 ft-lb | ASTM D5420 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |