Polymer Property : Gardner Impact = 28.2 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 28.2 J

@Thickness 3.18 mm,
Temperature 23.0 °C
20.8 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
PolyOne Maxxam™ FR PP FR 7C11 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D3029
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D3029
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Gardner Impact 28.2 J

@Temperature 23.0 °C
20.8 ft-lb

@Temperature 73.4 °F
ASTM D5420, GB
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA)
Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa..
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D5420
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic..
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D5420
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable..
Gardner Impact 28.2 J
20.8 ft-lb
ASTM D1709
Multibase Multi-Flex® TPE A 5009
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Gardner Impact 28.2 J

@Temperature -30.0 °C
20.8 ft-lb

@Temperature -22.0 °F
ASTM D3029
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro..
Gardner Impact 28.2 J

@Thickness 3.17 mm,
Temperature -30.0 °C
20.8 ft-lb

@Thickness 0.125 in,
Temperature -22.0 °F
Geometry GC; ASTM D5420
ExxonMobil PP7032E2 Impact Copolymer
Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit..
Gardner Impact 28.2 J

@Temperature 23.0 °C
20.8 ft-lb

@Temperature 73.4 °F
ASTM D3029
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap..
Gardner Impact >= 28.2 J
>= 20.8 ft-lb
ASTM D3029
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact >= 28.2 J
>= 20.8 ft-lb
ASTM D3029
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.