Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.6 J | 27.0 ft-lb | 0; ASTM D5420 |
Dow 334.03 Developmental Performance Polypropylene Polymer DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use app.. |
|||
Gardner Impact | 36.6 J | 27.0 ft-lb | 23; ASTM D5420 |
Dow 334.03 Developmental Performance Polypropylene Polymer DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use app.. |